Effect of thickness on structural properties of BixSb2-xTe3 thin films

Main Article Content

Hussain. M. Selman

Abstract

BixSb2-xTe3 alloys with different ratios of Bi (x=0, 0.1, 0.3, 0.5, and 2) have been prepared, Thin films of these alloys were prepared using thermal evaporation method under vacuum of 10-5 Torr on glass substrates at room temperature with different deposition rate (0.16, 0.5, 0.83) nm/sec for thickness (100, 300, 500) respectively. The X–ray diffraction measurements for BixSb2-xTe3 bulk and thin films indicate the polycrystalline structure with a strong intensity of peak of plane (015) preferred orientation with additional peaks, (0015) and (1010 ) reflections planes, which is meaning that all films present a very good texture along the (015) plane axis at different intensities for each thin film for different thickness. AFM measurements for the thin films of BixSb2-xTe3, show that the grain size and the average surface roughness decreases with increasing of the percentage Bi for different thickness.

Article Details

Section

Articles

How to Cite

1.
Selman HM. Effect of thickness on structural properties of BixSb2-xTe3 thin films. IJP [Internet]. 2019 May 29 [cited 2024 Dec. 24];17(41):15-28. Available from: https://ijp.uobaghdad.edu.iq/index.php/physics/article/view/451

Similar Articles

You may also start an advanced similarity search for this article.