Chemical spray pyrolysis technique was used at substrate temperature 250 ˚C with annealing temperature at 400 ˚C (for 1hour) to deposition tungsten oxide thin film with different doping concentration of Au nanoparticle (0, 10, 20, 30 and 40)% wt. on glass substrate with thickness about 100 nm. The structural, optical properties were investigated. The X-ray diffraction shows that the films at substrate temperature (250 ˚C) was amorphous while at annealing temperature have a polycrystalline structure with the preferred orientation of (200), all the samples have a hexagonal structure for WO3 and Au gold nanoparticles have a cubic structure. Atomic force microscopy (AFM) was used to characterize the morphology of the films. The optical properties of the films were studied using UV-Vis spectrophotometer within the wavelength in the range (300-1100) nm. The optical energy gap of the films was (2.80) eV for WO3 and it decreased at annealing temperature (400 ˚C) equal to (2.65) eV. And finally the optical constants such as refractive index, real and imaginary dielectrics, absorption coefficient, absorption, transmission, and extinction coefficient were investigated.

Article Details

How to Cite
1.
The effect of gold nanoparticles on WO3 thin film. IJP [Internet]. 2018 Oct. 1 [cited 2024 Mar. 29];16(36):11-28. Available from: https://ijp.uobaghdad.edu.iq/index.php/physics/article/view/22
Section
Articles

How to Cite

1.
The effect of gold nanoparticles on WO3 thin film. IJP [Internet]. 2018 Oct. 1 [cited 2024 Mar. 29];16(36):11-28. Available from: https://ijp.uobaghdad.edu.iq/index.php/physics/article/view/22

Similar Articles

You may also start an advanced similarity search for this article.